Polymer Property : Tensile Strength, Ultimate = 508 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.50 MPa

@Temperature 800 °C
508 psi

@Temperature 1470 °F
Pyrotek Firefly 800 Roller & Furnace Cladding Material
Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. F..