Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 38.6 MPa @Temperature 260 °C |
5600 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |
|||
Tensile Strength, Ultimate | 38.6 MPa @Temperature 260 °C |
5600 psi @Temperature 500 °F |
ASTM D 638 |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |