Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 614 MPa @Diameter 12.7 mm, Temperature 260 °C |
89100 psi @Diameter 0.500 in, Temperature 500 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Ultimate | 614 MPa @Temperature 204 °C |
89000 psi @Temperature 400 °F |
|
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability .. |