Tensile Strength, Ultimate 434 MPa

@Thickness 12.7 mm,
Temperature 760 °C
62900 psi

@Thickness 0.500 in,
Temperature 1400 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..