Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 643 MPa

@Thickness 9.50 mm,
Temperature 538 °C
93300 psi

@Thickness 0.374 in,
Temperature 1000 °F
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Tensile Strength, Ultimate 643 MPa

@Thickness 3.20 mm,
Temperature 538 °C
93300 psi

@Thickness 0.126 in,
Temperature 1000 °F
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..