Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 673 MPa

@Thickness 12.7 mm,
Temperature 427 °C
97600 psi

@Thickness 0.500 in,
Temperature 801 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Ultimate 673 MPa

@Thickness 2.40 mm,
Temperature 316 °C
97600 psi

@Thickness 0.0945 in,
Temperature 601 °F
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'..