Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 688 MPa @Thickness 12.7 mm, Temperature 427 °C |
99800 psi @Thickness 0.500 in, Temperature 801 °F |
|
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Tensile Strength, Ultimate | 688 MPa @Thickness 19.1 mm, Temperature 371 °C |
99800 psi @Thickness 0.752 in, Temperature 700 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |