Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 689 MPa

@Thickness 12.7 mm,
Temperature 25.0 °C
99900 psi

@Thickness 0.500 in,
Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Tensile Strength, Ultimate 689 MPa

@Thickness 4.00 mm,
Temperature 204 °C
99900 psi

@Thickness 0.157 in,
Temperature 399 °F
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Tensile Strength, Ultimate 689 MPa

@Thickness 63.5 mm,
Temperature 25.0 °C
99900 psi

@Thickness 2.50 in,
Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..