Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 707 MPa @Thickness 12.7 mm, Temperature 316 °C |
103000 psi @Thickness 0.500 in, Temperature 601 °F |
|
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |