Tensile Strength, Ultimate 492 MPa

@Temperature 23.0 °C
71400 psi

@Temperature 73.4 °F
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed
AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistance in the presence of chl..