Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 52.11 MPa @Temperature 100 °C, Time 605000 sec |
7558 psi @Temperature 212 °F, Time 168 hour |
Oven Aging |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Tensile Strength, Ultimate | 52.11 MPa @Temperature 100 °C, Time 2.42e+6 sec |
7558 psi @Temperature 212 °F, Time 672 hour |
Oven Aging |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Tensile Strength, Ultimate | 52.11 MPa @Temperature 70.0 °C, Time 2.42e+6 sec |
7558 psi @Temperature 158 °F, Time 672 hour |
Water Immersion |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |