Polymer Property : Tensile Strength, Ultimate = 76900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 530 MPa

@Thickness 203 - 305 mm
76900 psi

@Thickness 8.00 - 12.0 in
at center (L/T direction)
Alcoa QC-10® Aluminum Mold Alloy
Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-..
Tensile Strength, Ultimate 530 MPa

@Temperature 200 °C
76900 psi

@Temperature 392 °F
short term exposure
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us..