Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 814 MPa

@Thickness 9.50 - 25.4 mm,
Temperature 93.0 °C
118000 psi

@Thickness 0.374 - 1.00 in,
Temperature 199 °F
Haynes Hastelloy® S alloy, flat products
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Ultimate 814 MPa

@Temperature 23.0 °C
118000 psi

@Temperature 73.4 °F
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100)