Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 899 MPa @Thickness 12.7 mm, Temperature 25.0 °C |
130000 psi @Thickness 0.500 in, Temperature 77.0 °F |
As Welded, Base/Base Fracture |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |