Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 641 MPa

@Temperature 149 °C
93000 psi

@Temperature 300 °F
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability ..
Tensile Strength, Ultimate 641 MPa

@Thickness 25.4 mm
93000 psi

@Thickness 1.00 in
LT Direction
Alcoa 7055-T77511 Aluminum Extrusions
Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures..
Tensile Strength, Ultimate 641 MPa

@Temperature 260 °C
93000 psi

@Temperature 500 °F
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..