Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 647 MPa

@Diameter 12.7 mm,
Temperature 260 °C
93800 psi

@Diameter 0.500 in,
Temperature 500 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..