Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 654 MPa

@Thickness 12.7 mm,
Temperature 260 °C
94900 psi

@Thickness 0.500 in,
Temperature 500 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..