Tensile Modulus 0.00310 GPa

@Temperature -20.0 °C
0.450 ksi

@Temperature -4.00 °F
Gehman Rigidity; ASTM D1053
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr..