Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.075 GPa @Temperature 23.0 °C |
155.9 ksi @Temperature 73.4 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Tensile Modulus | 1.075 GPa @Temperature 23.0 °C |
155.9 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |