Mechanical Properties Metric English Comments
Tensile Modulus 1.70 GPa

@Temperature 23.0 °C
247 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Tensile Modulus 1.70 GPa

@Temperature 150 °C
247 ksi

@Temperature 302 °F
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Modulus 1.70 GPa

@Temperature 120 °C
247 ksi

@Temperature 248 °F
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
Tensile Modulus 1.70 GPa

@Temperature 60.0 °C
247 ksi

@Temperature 140 °F
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Modulus 1.70 GPa

@Temperature 120 °C
247 ksi

@Temperature 248 °F
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Tensile Modulus 1.70 GPa

@Temperature 150 °C
247 ksi

@Temperature 302 °F
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Modulus 1.70 GPa

@Temperature 150 °C
247 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro..
Tensile Modulus 1.70 GPa

@Temperature 120 °C
247 ksi

@Temperature 248 °F
LATI Latilon 30D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Tensile Modulus 1.70 GPa

@Temperature 23.0 °C
247 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..