Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.777 GPa @Temperature 60.0 °C |
257.7 ksi @Temperature 140 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66