Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.2 GPa @Temperature -40.0 °C |
1620 ksi @Temperature -40.0 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |