Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.86 GPa @Thickness 0.102 mm |
1140 ksi @Thickness 0.00400 in |
RT; ASTM D638 |
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a .. |