Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 132.3 GPa @Temperature 24.0 °C |
19190 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel |