Polymer Property : Tensile Modulus = 14.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 14.8 GPa

@Temperature 60.0 °C
2150 ksi

@Temperature 140 °F
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..