Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.3 GPa @Temperature 150 °C |
1490 ksi @Temperature 302 °F |
|
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |