Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.9 GPa @Temperature 90.0 °C |
2450 ksi @Temperature 194 °F |
|
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |