Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 18.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 18.0 GPa

@Temperature 23.0 °C
2610 ksi

@Temperature 73.4 °F
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 18.0 GPa

@Temperature 60.0 °C
2610 ksi

@Temperature 140 °F
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 18.0 GPa

@Temperature 23.0 °C
2610 ksi

@Temperature 73.4 °F
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 18.0 GPa

@Temperature 23.0 °C
2610 ksi

@Temperature 73.4 °F
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Tensile Modulus 18.0 GPa

@Temperature 23.0 °C
2610 ksi

@Temperature 73.4 °F
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: ..
Tensile Modulus 18.0 GPa

@Temperature 60.0 °C
2610 ksi

@Temperature 140 °F
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 18.0 GPa

@Temperature 23.0 °C
2610 ksi

@Temperature 73.4 °F
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Tensile Modulus 18.0 GPa

@Temperature 177 °C
2610 ksi

@Temperature 351 °F
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F161; Fiber: 450-1/2Information provided by HexCel
Tensile Modulus 18.0 GPa

@Temperature 150 °C
2610 ksi

@Temperature 302 °F
ISO 527-1
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound
BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri..