Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 22.1 GPa @Temperature 71.1 °C |
3200 ksi @Temperature 160 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Modulus | 22.1 GPa @Temperature 93.3 °C |
3200 ksi @Temperature 200 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Modulus | 22.1 GPa @Temperature 21.1 °C |
3200 ksi @Temperature 70.0 °F |
0° Direction, Wet; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Modulus | 22.1 GPa @Temperature 71.1 °C |
3200 ksi @Temperature 160 °F |
0° Direction, Dry; Autoclave, 50 psi, 90min; ASTM D638 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Tensile Modulus | 22.1 GPa @Temperature 82.2 °C |
3200 ksi @Temperature 180 °F |
Wet; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Tensile Modulus | 22.1 GPa @Temperature 149 °C |
3200 ksi @Temperature 300 °F |
Dry; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Tensile Modulus | 22.1 GPa @Temperature 23.0 °C |
3210 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |