Tensile Modulus 15.8 GPa

@Temperature 23.0 °C
2290 ksi

@Temperature 73.4 °F
LATI Latamid 12 H2 K/30 PA 12, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 12 (PA12) based compound. Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 15.8 GPa

@Temperature 60.0 °C
2290 ksi

@Temperature 140 °F
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Tensile Modulus 15.8 GPa

@Temperature 177 °C
2290 ksi

@Temperature 351 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber
Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel