Tensile Modulus 1.60 GPa

@Temperature 23.0 °C
232 ksi

@Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Crastin® ST820 BK503 PBT  (Unverified Data**)
Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 1.60 GPa

@Temperature 23.0 °C
232 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Crastin® ST820 BK503 PBT  (Unverified Data**)
Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 1.60 GPa

@Temperature 120 °C
232 ksi

@Temperature 248 °F
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Tensile Modulus 1.60 GPa

@Temperature 60.0 °C
232 ksi

@Temperature 140 °F
LATI Latan 23UV POM
Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..
Tensile Modulus 1.60 GPa

@Temperature 120 °C
232 ksi

@Temperature 248 °F
LATI Latilon 28D PC
Polycarbonate (PC). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability. Very good surface appearanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 1.60 GPa

@Temperature 120 °C
232 ksi

@Temperature 248 °F
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Tensile Modulus 1.60 GPa

@Thickness 1.00 - 6.00 mm
232 ksi

@Thickness 0.0394 - 0.236 in
ASTM D638
CPC - Vycom CELTEC® Expanded Rigid foam PVC board
Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface..
Tensile Modulus 1.60 GPa

@Temperature 60.0 °C
232 ksi

@Temperature 140 °F
LATI Later 4-V0 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L..
Tensile Modulus 1.60 GPa

@Temperature 150 °C
232 ksi

@Temperature 302 °F
LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; La..