Polymer Property : Tensile Modulus = 2550 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 17.6 GPa

@Temperature 23.0 °C
2550 ksi

@Temperature 73.4 °F
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 17.6 GPa

@Temperature 90.0 °C
2550 ksi

@Temperature 194 °F
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..