Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.86 GPa @Temperature 149 °C |
270 ksi @Temperature 300 °F |
|
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor .. |