Polymer Property : Tensile Modulus = 29.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 29.0 GPa

@Temperature 23.0 °C
4210 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 29.0 GPa

@Temperature 250 °C
4210 ksi

@Temperature 482 °F
ISO 527-1
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex..