Mechanical Properties Metric English Comments
Tensile Modulus 31.0 GPa

@Temperature 120 °C
4500 ksi

@Temperature 248 °F
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..