Polymer Property : Tensile Modulus = 310 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.14 GPa

@Temperature 149 °C
310 ksi

@Temperature 300 °F
Master Bond EP46HT Epoxy Adhesive for Structural Bonding
Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f..