Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 40.0 GPa @Temperature 23.9 °C |
5800 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D3039 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Tensile Modulus | 40.0 GPa @Temperature 120 °C |
5800 ksi @Temperature 248 °F |
Dry; EN2561 |
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ.. |
|||
Tensile Modulus | 40.0 GPa @Temperature 180 °C |
5800 ksi @Temperature 356 °F |
Dry; EN2561 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |