Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 303 GPa @Temperature 23.0 °C |
43900 ksi @Temperature 73.4 °F |
0° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, G80-600 Fiber Information provided by HexCel |