Mechanical Properties Metric English Comments
Tensile Modulus 3.284 GPa

@Temperature 150 °C
476.3 ksi

@Temperature 302 °F
ISO 527
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers