Tensile Modulus 3.45 GPa

@Temperature 90.0 °C
500 ksi

@Temperature 194 °F
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..