Mechanical Properties Metric English Comments
Tensile Modulus 3.50 GPa

@Thickness 0.100 mm
508 ksi

@Thickness 0.00394 in
MD; ISO 527
Victrex® APTIV® 2102-100M Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled
APTIV® 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV ..
Tensile Modulus 3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Tensile Modulus 3.50 GPa

@Temperature 23.0 °C
508 ksi

@Temperature 73.4 °F
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Modulus 3.50 GPa

@Temperature 60.0 °C
508 ksi

@Temperature 140 °F
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Modulus 3.50 GPa

@Temperature 23.0 °C
508 ksi

@Temperature 73.4 °F
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle..
Tensile Modulus 3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi..
Tensile Modulus 3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica..
Tensile Modulus 3.50 GPa

@Temperature 150 °C
508 ksi

@Temperature 302 °F
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Tensile Modulus 3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail..
Tensile Modulus 3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant
High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid..
Tensile Modulus 3.50 GPa

@Temperature 23.0 °C
508 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® BM70G15HSLR BK537 Nylon 66
Zytel® BM70G15HSLR BK537 is a 15% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers