Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 39.0 GPa @Temperature 90.0 °C |
5660 ksi @Temperature 194 °F |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |