Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 42.0 GPa @Temperature 60.0 °C |
6090 ksi @Temperature 140 °F |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |