Mechanical Properties Metric English Comments
Tensile Modulus 62.7 GPa

@Temperature 210 °C
9100 ksi

@Temperature 410 °F
Wet, 0° Direction; SACMA SRM 4R-94
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Tensile Modulus 62.7 GPa

@Temperature 71.0 °C
9090 ksi

@Temperature 160 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric
Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel