Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.50 GPa @Temperature 150 °C |
653 ksi @Temperature 302 °F |
|
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 90.0 °C |
653 ksi @Temperature 194 °F |
|
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 60.0 °C |
653 ksi @Temperature 140 °F |
|
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 120 °C |
653 ksi @Temperature 248 °F |
|
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 60.0 °C |
653 ksi @Temperature 140 °F |
|
LATI Latene® AG7H G/30 PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers. Good thermal propertiesAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 150 °C |
653 ksi @Temperature 302 °F |
|
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 120 °C |
653 ksi @Temperature 248 °F |
|
LATI Latigloss 62 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 6 (PA6). Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Ameri.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 120 °C |
653 ksi @Temperature 248 °F |
|
LATI Latilon 28D G/20-V0 PC, 20% Glass Fiber Reinforced, Flame Retardant Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab.. |