Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.476 GPa @Temperature 120 °C |
69.0 ksi @Temperature 248 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |