Mechanical Properties Metric English Comments
Tensile Modulus 5.00 GPa

@Temperature 150 °C
725 ksi

@Temperature 302 °F
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low..
Tensile Modulus 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm..
Tensile Modulus 5.00 GPa

@Temperature 150 °C
725 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. improved G.W.F.I. compared to standard product.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Tensile Modulus 5.00 GPa

@Temperature 90.0 °C
725 ksi

@Temperature 194 °F
LATI Latamid 66 VH2 G/30 PA 66, 30% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Improved thermal stabilization. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In..
Tensile Modulus 5.00 GPa

@Temperature 150 °C
725 ksi

@Temperature 302 °F
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 5.00 GPa

@Temperature 120 °C
725 ksi

@Temperature 248 °F
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Potentially suitable for food/medical contact application. Availab..
Tensile Modulus 5.00 GPa

@Temperature 90.0 °C
725 ksi

@Temperature 194 °F
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail..
Tensile Modulus 5.00 GPa

@Temperature 60.0 °C
725 ksi

@Temperature 140 °F
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..