Polymer Property : Tensile Modulus = 8.77 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.77 GPa

@Temperature 200 °C
1270 ksi

@Temperature 392 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree..
Tensile Modulus 8.77 GPa

@Temperature 200 °C
1270 ksi

@Temperature 392 °F
2; ISO 527-2
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber
Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional ..