Polymer Property : Tensile Modulus = 9800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 67.6 GPa

@Temperature 23.9 °C
9800 ksi

@Temperature 75.0 °F
0° Direction, Dry, 365° Oven Cured; ASTM D3039
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Tensile Modulus 67.6 GPa

@Temperature 77.0 °C
9800 ksi

@Temperature 171 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Tensile Modulus 67.6 GPa

@Temperature 200 °C
9800 ksi

@Temperature 392 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel