Polymer Property : Compressive Strength = 0.1094 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.1094 MPa

@Strain 25.0 %
15.86 psi

@Strain 25.0 %
ASTM D3575
Sekisui PIOCELAN SP-50E Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..